CRUCIBLE 440C (AISI 440C) |
![]() |
|||||||||||||||||||||||||||||||||||
Crucible 440C is a heat treatable stainless steel, designed for a combination of high wear resistance and moderate corrosion resistance in mild environments. |
||||||||||||||||||||||||||||||||||||
|
|
|||||||||||||||||||||||||||||||||||
|
||||||||||||||||||||||||||||||||||||
|
||||||||||||||||||||||||||||||||||||
|
||||||||||||||||||||||||||||||||||||
![]() |
||||||||||||||||||||||||||||||||||||
Surface Treatments Nitriding decreases the corrosion resistance of stainless steels, and is not generally recommended for this grade. Because of the limitations of tempering between 800 and 1100F, surface treatments for 440C should be limited to those compatible with tempering temperatures under 800F. Annealing A. Heat to 1650F, hold two hours, cool slowly (25F/hour maximum) to 1200F, then air cool. Or B. Heat to 1600F, hold two hours, cool to 1300F, hold 4 hours, then air cool. Typical annealed hardness: 217/255 BHN. Stress Relieving Annealed Material: Heat to 1200/1250F, hold two hours, cool in still air. Hardened Material: Heat to 25F below original tempering temperature, hold two hours, cool in still air. Welding Use type 440C or 420 filler material. Annealed Material: Preheat to 600/800F. Maintain above 600F during welding. Reanneal or temper 1300F 4 hours. Hardened Material: Preheat to 25F below original tempering temperature (400F minimum). Maintain above 400F during welding. Cool to 150F after welding. Temper 25F below original tempering temperature (400F) minimum. Physical Properties Modulus of Elasticity ..............................................................30 psi x 106 Density .......................................................................................0.278 lb/in3 Thermal Conductivity ...................200F............................ 14 BTU/hr/ft/°F Thermal Expansion RT-200F ..................................................................5.7 X 10-6 in./in./°F RT-600F ................................................................. 6.0 X 10-6 in./in./°F |
||||||||||||||||||||||||||||||||||||
|